型号 | DPT10016-HQ | |||
主弧 | 水电一体 | 冷却 | 主弧维弧循环冷却 | |
钨极-工件 | 负极-正极 | 离子气 | 0.3-3L/min | |
钨针型号 | 2.4 | 保护气 | 5-25L/min | |
电弧电压 | 90V | 喷嘴冷却 | 直接水冷 | |
焊接电流 | 30-100A 100%暂载率 | 喷嘴孔径 | 2.4 | |
维弧 | 气电一体 | 电缆长度 | 标配4M (可定制) | |
钨极-喷嘴 | 负极-正极 | |||
维弧电流 | 3-20A 100% 暂载率 | |||
送粉类型 | 保护罩聚集型送粉 | |||
送粉量 | 最大50g/min | |||
送粉气 | 1.0-3.0L/min | |||
粉末类型 | 金属粉末 | |||
粉末颗粒 | 70-200um | |||
送粉气路 | 单气路进入 |
model | DPT10016-HQ | |||
Main arc | Hydropower integration | cooling | Main arc cooling | |
Tungsten electrode workpiece | Negative positive | Ion gas | 0.3-3L/min | |
Tungsten needle model | 2.4 | Protective gas | 5-25L/min | |
arc voltage | 90V | Nozzle cooling | Direct water cooling | |
welding current | 30-100a 100% temporary load rate | Nozzle aperture | 2.4 | |
Dimensional arc | Integration of gas and electricity | Cable length | Standard 4m (customizable) | |
Tungsten electrode nozzle | Negative positive | |||
Dimensional arc current | 3-20a 100% temporary load rate | |||
Powder feeding type | Protective cover aggregate powder feeding | |||
Powder feeding capacity | Max. 50g / min | |||
Powder feeding gas | 1.0-3.0L/min | |||
Powder type | metal powder | |||
Powder particles | 70-200um | |||
Powder feeding gas path | Single gas path entry |
Now the lose efficiency of mining machinery is mainly caused by friction and wear that results in the huge loss of people's lives and property, the sum is up to hundreds of millions of dollars. Due to the poor working condition and the seve...
Petroleum industry wearing parts: valve, hydraulic rod, valve core, hydraulic cylinder, gate, drill, etc., using Shanghai Duo Mu plasma hardfacing machine can effectively repair petroleum equipment, wear resistance and corrosion resistance, ...
In the process of smelting, the deterioration of machine is due to the natural environment and the external force, such as strike, fatigue and so on. In addition to this those would lead to phenomenon of being defaced of machine, including ...
Powder surfacing machine is a metal surface modification equipment independently developed by Duomu Industry, which has completely independent intellectual property rights. The surfacing equipment process is one of the effective technical me...
Powder surfacing machine is a metal surface modification equipment independently developed by Duomu Industrial Company, which has completely independent intellectual property rights. Plasma surfacing technology is mainly used to improve the ...
The powder surfacing machine uses a plasma arc high-energy density beam as the welding heat source. The powder surfacing machine has the characteristics of energy concentration, high production efficiency, fast welding speed, small stress an...
The editor of Duomu Industry summarized several protective measures for using powder surfacing machine: Prevent electric shock. The no-load voltage of powder surfacing machine and cutting power supply is relatively high, especially when it i...