Your current location: Home > Solution > Mine

Shanghai Duomuji Industrial Co., Ltd. is a comprehensive high-tech industrial company rising in the economic tide, specializing in the development, production and sales of high-end power supply and precision welding equipment. The precise ion welding (Plasma), precise arc welding machine (Fine TIG) and plasma surfacing welding machine (PTA) developed by the company are widely used in many fields of industrial production such as automobile, ship, aviation, petrochemical industry, etc., and solve many welding and repair problems for customers.

Product Application

Pick scheme

Machine name:

Product Description:

Features of CNC surfacing machine tools:

1 digital control system, multi-axis linkage control.
Step motor (optional servo motor) is used for stable operation and high precision.
3. The degree of automation is high, and the surfacing process is completed once, with high efficiency.
The four systems are stable and have strong anti-interference ability.
Five cutters and round workpieces of various types can be hardfaced.
6 small current surfacing has little heat influence, and the pick of brazing alloy head can also be smoothly surfacing, without affecting brazing and falling off.

Product Description

Professional pick surfacing, choose Duomu!
Details of product parameters of Duomu DML-03 Stack welding machine

Main technical parameters and models DML-03
Pulse welding Continuous welding
Arc current IP (a) 3-20 3-20
Welding current I1 (a) 2-300 2-300
Base current I2 (a) 2-110  
Current rise time T3 (s) 0-2.0 0-2.0
Current drop time T4 (s) 0-2.0 0-2.0
Pulse welding time T1 (MS) 1-999  
Welding interval T2 (MS) 10-990  
Gas protection time (s) 1.0-20.0 1-20.0
Input voltage (V) Three phase 380V, 50 Hz AC
Rated input power capacity (kVA) eight
Output current regulation range (a) 1-300
Load duration rate (%) 60%
Ion gas flow rate (L / min) 0.2-1
Protective gas flow (L / min) 1-12
Weight (kg) eighty-two
Overall dimension (mm) 695*375*665

The company always adheres to the tenet of "high-tech products, high-quality products, high-efficiency services", meticulously creates "more integrity, more professional trees", constantly improves the core competitiveness of the enterprise, and is committed to becoming the industry's leading team.
Pick is the key part of shearer, digger and other machinery. The plasma powder surfacing cladding of pick is a layer of high hardness and wear-resistant alloy layer on the front working face of the pick, which can prolong the service life of the pick and improve the working efficiency. At the same time, excellent   The non spark effect is basically achieved when the alloy layer is in friction with hard materials such as rocks, which greatly ensures the operation safety of high gas mine. Therefore, the non spark pick of surfacing has become the first product of modern coal mine production.

Other solution cases


dial navigation search