Configuration items |
Model and brand |
Description of main parameters |
Arc voltage tracking |
Multi wood integration |
|
Current communication |
485 communication |
|
touch screen |
Wellington |
7-inch screen tk6071iq |
Control system |
Mitsubishi, Japan |
FX series PLC |
Console |
Multiwood manufacturing |
Mobile control platform, handheld touch control box |
Electrical components |
chint |
|
Transverse mechanism |
Research and control stepping motor |
Effective stroke 1300 mm |
Lifting mechanism |
Research and control stepping motor |
Effective stroke 1500mm |
Spindle motor |
Xinjie servo motor |
The rotation speed is 0.01r/min ~ 2.5r/min |
Welding positioner |
DHB-12 |
Rated load 1200 kg |
Welding wiggler |
BDQ-80 |
Swing speed 1-30 mm / S The swing distance is 3-60 mm |
Three jaw chuck |
K11-500C |
The clamping range is 25-500 mm |
Reference footprint |
It is 3500 mm long, 1800 mm wide and 2400 mm high. |